KISE Journal of Korean Institute of Surface Engineering 2003;36(4):317-323. Published online: Nov, 30, -0001
The effect of additives such as complexing agents, stabilzers and boric acid on the bath stability and the deposition rate of electroless black Ni-Zn plating has been examined. The deposits obtained became black and showed an amorphous structure. The sign
키워드 Black Ni-Zn;Electroless plating;Additives;Deposition rate;Stability;