In this study, in order to improve corrosion resistance and wear resistance of aluminum, surface treatment was made by anodizing with oxalic acid solution and sealing with nano-diamond powder. Average size of nano-diamond powder was 30nm. Anodizing with o
키워드 Anodizing;Nano-diamond powder;Sealing treatment;Corrosion resistance and wear resistance;