KISE Journal of Korean Institute of Surface Engineering 2018;51(6):354-359. Published online: Nov, 30, -0001
DOI : 10.5695/JKISE.2018.51.6.354
NaCl-induced hot corrosion behavior of ASTM T22 (Fe-2.25Cr-1Mo), T91 (Fe-9Cr-1Mo), T92 (Fe-9Cr-1.8W-0.5Mo), 347HFG (Fe-18-Cr-11Ni), and 310H (Fe-25Cr-19Ni) steels was studied after spraying NaCl on the surface. During corrosion at
키워드 Fe-Cr steel;Stainless steel;Hot corrosion;NaCl salt;