KISE Journal of Korean Institute of Surface Engineering 2022;55(5):273-283. Published online: Nov, 14, 2022
DOI : 10.5695/JSSE.2022.55.5.273
Al6061 aluminum alloy specimens were exposed to atmospheric conditions for maximum 24 months. 24-month exposure specimen showed some more frequent and larger size of corrosion products and pitting on the surface compared with the 12-month exposure specime
키워드 Aluminum alloy; Al6061; Atmospheric corrosion; pitting corrosion; Intergranular corrosion.