KISE Journal of Korean Institute of Surface Engineering 2002;35(5):273-278. Published online: Nov, 30, -0001
We oxidized pure titanium by anodizing oxidation process in the range of 590V, within 1.5A, 30seconds. we investigated color evolution with a spectrophotometer. Surface images and surface roughness were characterized by an optical microscope and an atomic
키워드 Titanium;Titanium oxide;Anodized oxidation;Lightness;